SUM22L chemical composition and mechanical properties
● Chemical Composition: Carbon C: ≤ 0.13 Silicon Si: ≤ 0.15 Manganese Mn: 0.70 ~ 1.00 Sulfur S: 0.24 ~ 0.33 Phosphorus P: 0.07 ~ 0.12 Lead Pb: 0.10 ~ 0.35 ● mechanical properties: Tensile strength σb (MPa): (hot-rolled) 390 to 540; (cold drawn) steel thickness or diameter of 8 to 20: 530 to 755;> 20
30 to 30 hours: 510 to 735;>: 490 to 685 Elongation δ5 (%): (hot-rolled) ≥ 22; (cold rolled) ≥ 7.0 Reduction of area ψ (%): (hot-rolled) ≥ 36 Hardness: (hot) ≤ 170HB; (cold-drawn) 152 ~ 217HB ● Delivery status: hot-rolled or cold-drawn state delivery, delivery status should be specified in the contract. |